New Screening Study: Delamination under Control
A new series of studies has once again demonstrated the effectiveness of SCHOTT Vials Delamination Controlled (DC). These pharmaceutical vials have a particularly high chemical durability and are therefore less susceptible to delamination. SCHOTT has had this property confirmed in various storage studies. First, substances were used that have already caused product recalls due to delamination. In a second series of studies, the question of how effectively buffer systems can be stored in the new bottle was examined more closely. The result: if the respective substances were stored in SCHOTT Vials DC, the vials remained stable and no glass delamination was observed. A detailed presentation of results was published in the November/December 2016 issue of the PDA Journal.