SF10

Glass Code:  728284.428

A classic glass type with lead oxide as an essential component for outstanding optical properties.

Find more information in the tabs below or on our website.

Compare glass types with our Interactive Abbe Diagram.

optical glass klein 4zu3.jpg
Characteristics
nd 1.72825 νd 28.41
ne 1.73430 νe 28.19
nF-nC 0.025633 nF'-nC' 0.026051
Sign in to choose your product

As a registered user in our shop you enjoy many advantages

  • Simply order
  • Stock overview
  • Simple profile management
Need help or a quote?
CONTACT OUR SUPPORT
Article Details
SCHOTT
Article
Glass type
L
W
T
DIA
Step
nd
Step
vd
nd
vd
Weight
 
 
Technical Details
Refractive Indices
Characteristics λ [nm]
n2,325.4 2,325.4 1.68218
n1,970.1 1,970.1 1.68750
n1,529.6 1,529.6 1.69378
n1,060.0 1,060.0 1.70227
nt 1,014.0 1.70345
ns 852.1 1.70887
nr 706.5 1.71681
nC 656.3 1.72085
nC' 643.8 1.72200
Characteristics λ [nm]
n632.8 632.8 1.72309
nD 589.3 1.72803
nd 587.6 1.72825
ne 546.1 1.73430
nF 486.1 1.74648
nF' 480.0 1.74805
ng 435.8 1.76198
nh 404.7 1.77579
ni 365.0
Characteristics λ [nm]
n334.1 334.1
n312.6 312.6
n296.7 296.7
n280.4 280.4
n248.3 248.3
Internal Transmittance
Characteristics λ [nm]
τ25/2500 2,500 0.690
τ25/2325 2,325 0.760
τ25/1970 1,970 0.920
τ25/1530 1,530 0.987
τ25/1060 1,060 0.997
τ25/700 700 0.995
τ25/660 660 0.993
τ25/620 620 0.993
τ25/580 580 0.995
τ25/546 546 0.995
τ25/500 500 0.989
τ25/460 460 0.978
τ25/436 436 0.961
τ25/420 420 0.920
τ25/405 405 0.790
τ25/400 400 0.690
τ25/390 390 0.370
τ25/380 380 0.060
τ25/370 370
τ25/365 365
τ25/350 350
τ25/334 334
τ25/320 320
τ25/310 310
τ25/300 300
τ25/290 290
τ25/280 280
τ25/270 270
τ25/260 260
τ25/250 250
Characteristics λ [nm]
τ10/2500 2,500 0.862
τ10/2325 2,325 0.896
τ10/1970 1,970 0.967
τ10/1530 1,530 0.995
τ10/1060 1,060 0.999
τ10/700 700 0.998
τ10/660 660 0.997
τ10/620 620 0.997
τ10/580 580 0.998
τ10/546 546 0.998
τ10/500 500 0.996
τ10/460 460 0.991
τ10/436 436 0.984
τ10/420 420 0.967
τ10/405 405 0.910
τ10/400 400 0.862
τ10/390 390 0.672
τ10/380 380 0.360
τ10/370 370 0.080
τ10/365 365 0.020
τ10/350 350
τ10/334 334
τ10/320 320
τ10/310 310
τ10/300 300
τ10/290 290
τ10/280 280
τ10/270 270
τ10/260 260
τ10/250 250
Partial Dispersion
Characteristics
Ps,t 0.2111
PC,s 0.4674
Pd,C 0.2888
Pe,d 0.2361
Pg,F 0.6046
Pi,h
P's,t 0.2077
P'C',s 0.5042
P'd,C' 0.2399
P'e,d 0.2323
P'g,F' 0.5346
P'i,h
Characteristics
ΔPC,t -0.0012
ΔPC,s -0.0017
ΔPF,e 0.0017
ΔPg,F 0.0085
ΔPi,g