RG1000

- SCHOTT
- RG1000 - RG1000
- 厚度
- 3.0
- 反射系数
- 0.9133
λ [nm] | |
---|---|
200 | < 10⁻³ |
210 | < 10⁻³ |
220 | < 10⁻³ |
230 | < 10⁻³ |
240 | < 10⁻³ |
250 | < 10⁻³ |
260 | < 10⁻³ |
270 | < 10⁻³ |
280 | < 10⁻³ |
290 | < 10⁻³ |
300 | < 10⁻³ |
310 | < 10⁻³ |
320 | < 10⁻³ |
330 | < 10⁻³ |
340 | < 10⁻³ |
350 | < 10⁻³ |
360 | < 10⁻³ |
370 | < 10⁻³ |
380 | < 10⁻³ |
390 | < 10⁻³ |
400 | < 10⁻³ |
410 | < 10⁻³ |
420 | < 10⁻³ |
430 | < 10⁻³ |
440 | < 10⁻³ |
450 | < 10⁻³ |
460 | < 10⁻³ |
470 | < 10⁻³ |
480 | < 10⁻³ |
490 | < 10⁻³ |
λ [nm] | |
---|---|
500 | < 10⁻³ |
510 | < 10⁻³ |
520 | < 10⁻³ |
530 | < 10⁻³ |
540 | < 10⁻³ |
550 | < 10⁻³ |
560 | < 10⁻³ |
570 | < 10⁻³ |
580 | < 10⁻³ |
590 | < 10⁻³ |
600 | < 10⁻³ |
610 | < 10⁻³ |
620 | < 10⁻³ |
630 | < 10⁻³ |
640 | < 10⁻³ |
650 | < 10⁻³ |
660 | < 10⁻³ |
670 | < 10⁻³ |
680 | < 10⁻³ |
690 | < 10⁻³ |
700 | < 10⁻³ |
710 | < 10⁻³ |
720 | < 10⁻³ |
730 | < 10⁻³ |
740 | < 10⁻³ |
750 | < 10⁻³ |
760 | < 10⁻³ |
770 | < 10⁻³ |
780 | < 10⁻³ |
790 | < 10⁻³ |
λ [nm] | |
---|---|
800 | < 10⁻³ |
810 | < 10⁻³ |
820 | < 10⁻³ |
830 | 0.002 |
840 | 0.003 |
850 | 0.007 |
860 | 0.013 |
870 | 0.022 |
880 | 0.036 |
890 | 0.052 |
900 | 0.077 |
910 | 0.107 |
920 | 0.141 |
930 | 0.182 |
940 | 0.225 |
950 | 0.273 |
960 | 0.318 |
970 | 0.368 |
980 | 0.413 |
990 | 0.461 |
1,000 | 0.503 |
1,010 | 0.546 |
1,020 | 0.585 |
1,030 | 0.619 |
1,040 | 0.653 |
1,050 | 0.682 |
1,060 | 0.708 |
1,070 | 0.732 |
1,080 | 0.754 |
1,090 | 0.773 |
λ [nm] | |
---|---|
1,100 | 0.792 |
1,110 | 0.808 |
1,120 | 0.823 |
1,130 | 0.835 |
1,140 | 0.846 |
1,150 | 0.856 |
1,160 | 0.866 |
1,170 | 0.874 |
1,180 | 0.882 |
1,190 | 0.888 |
1,200 | 0.894 |
1,250 | 0.918 |
1,300 | 0.934 |
1,350 | 0.944 |
1,400 | 0.952 |
1,450 | 0.958 |
1,500 | 0.964 |
1,550 | 0.969 |
1,600 | 0.972 |
1,650 | 0.975 |
1,700 | 0.976 |
1,750 | 0.977 |
1,800 | 0.976 |
1,850 | 0.975 |
1,900 | 0.973 |
1,950 | 0.971 |
2,000 | 0.969 |
2,050 | 0.966 |
2,100 | 0.962 |
2,150 | 0.955 |
λ [nm] | |
---|---|
2,200 | 0.944 |
2,250 | 0.934 |
2,300 | 0.932 |
2,350 | 0.928 |
2,400 | 0.922 |
2,450 | 0.914 |
2,500 | 0.905 |
2,550 | 0.896 |
2,600 | 0.886 |
2,650 | 0.874 |
2,700 | 0.837 |
2,750 | 0.572 |
2,800 | 0.446 |
2,850 | 0.424 |
2,900 | 0.414 |
2,950 | 0.394 |
3,000 | 0.370 |
3,050 | 0.337 |
3,100 | 0.301 |
3,150 | 0.264 |
3,200 | 0.230 |
3,250 | 0.201 |
3,300 | 0.175 |
3,350 | 0.151 |
3,400 | 0.130 |
3,450 | 0.117 |
3,500 | 0.109 |
3,550 | 0.103 |
3,600 | 0.099 |
3,650 | 0.098 |
λ [nm] | |
---|---|
3,700 | 0.098 |
3,750 | 0.100 |
3,800 | 0.104 |
3,850 | 0.108 |
3,900 | 0.114 |
3,950 | 0.118 |
4,000 | 0.116 |
4,050 | 0.109 |
4,100 | 0.098 |
4,150 | 0.086 |
4,200 | 0.072 |
4,250 | 0.059 |
4,300 | 0.043 |
4,350 | 0.029 |
4,400 | 0.018 |
4,450 | 0.009 |
4,500 | 0.003 |
4,550 | 0.001 |
4,600 | < 10⁻³ |
4,650 | < 10⁻³ |
4,700 | < 10⁻³ |
4,750 | < 10⁻³ |
4,800 | < 10⁻³ |
4,850 | < 10⁻³ |
4,900 | < 10⁻³ |
4,950 | < 10⁻³ |
5,000 | < 10⁻³ |
5,050 | < 10⁻³ |
5,100 | < 10⁻³ |
5,150 | < 10⁻³ |
反射系数 | |
---|---|
Pd | 0.913 |
参考厚度 | |
---|---|
d [mm] | 3 |
承诺光谱值 | |
---|---|
λs (τi = 0.00001) [nm] | 730 |
λc (τi = 0.5) [nm] | 1000 ± 6 |
λp1 (τi = 0.92) [nm] | 1300 |
折射率 n |
---|
nF (486.1 nm) = 1.548 |
nh (404.7 nm) = 1.558 |
ng (435.8 nm) = 1.554 |
ns (852.1 nm) = 1.532 |
ne (546.1 nm) = 1.543 |
nd (587.6 nm) = 1.541 |
色度评估
光源 | A(Planck T = 2347K) | ||
---|---|---|---|
d [mm] | 1 | 2 | 3 |
x | |||
y | |||
Y | |||
λd [nm] | |||
Pe |
光源 | Planck T = 3200 K | ||
---|---|---|---|
d [mm] | 1 | 2 | 3 |
x | |||
y | |||
Y | |||
λd [nm] | |||
Pe |
光源 | D65 (TC = 6504 K) | ||
---|---|---|---|
d [mm] | 1 | 2 | 3 |
x | |||
y | |||
Y | |||
λd [nm] | |||
Pe |
密度 | |
---|---|
p [g/cm3] | 2.73 |
气泡含量 | |
---|---|
气泡等级 | 3 |
玻转温度 | |
---|---|
Tg [°C] | 476 |
温度系数 | |
---|---|
Tk [nm/°C] | 0.41 |
耐化学性 | |
---|---|
耐污性 | 0 |
耐酸性 | 1.0 |
耐碱性 | 1.0 |
热膨胀 | |
---|---|
α-30°C/+70°C [10-6/K] | 9 |
α20°C/300°C [10-6/K] | 10.23 |
α20°C/200°C [10-6/K] |