BG26

承诺光谱值 | |
---|---|
τi (450nm) | ≥0.98 |
τi (633nm) | ≤0.79 |
τi (800nm) | ≤0.62 |
- SCHOTT
- BG26 - BG26
- 厚度
- 1.0
- 反射系数
- 0.9213
λ [nm] | |
---|---|
200 | |
210 | |
220 | |
230 | |
240 | |
250 | |
260 | |
270 | |
280 | < 10⁻³ |
290 | 0.005 |
300 | 0.079 |
310 | 0.314 |
320 | 0.595 |
330 | 0.785 |
340 | 0.888 |
350 | 0.940 |
360 | 0.964 |
370 | 0.977 |
380 | 0.982 |
390 | 0.986 |
400 | 0.989 |
410 | 0.990 |
420 | 0.991 |
430 | 0.992 |
440 | 0.992 |
450 | 0.993 |
460 | 0.993 |
470 | 0.993 |
480 | 0.991 |
490 | 0.989 |
λ [nm] | |
---|---|
500 | 0.985 |
510 | 0.979 |
520 | 0.971 |
530 | 0.960 |
540 | 0.946 |
550 | 0.931 |
560 | 0.913 |
570 | 0.893 |
580 | 0.871 |
590 | 0.848 |
600 | 0.824 |
610 | 0.800 |
620 | 0.776 |
630 | 0.752 |
640 | 0.729 |
650 | 0.707 |
660 | 0.687 |
670 | 0.668 |
680 | 0.651 |
690 | 0.636 |
700 | 0.624 |
710 | 0.611 |
720 | 0.601 |
730 | 0.593 |
740 | 0.586 |
750 | 0.580 |
760 | 0.576 |
770 | 0.572 |
780 | 0.570 |
790 | 0.569 |
λ [nm] | |
---|---|
800 | 0.568 |
810 | 0.569 |
820 | 0.570 |
830 | 0.572 |
840 | 0.575 |
850 | 0.578 |
860 | 0.582 |
870 | 0.586 |
880 | 0.591 |
890 | 0.596 |
900 | 0.603 |
910 | 0.609 |
920 | 0.616 |
930 | 0.623 |
940 | 0.630 |
950 | 0.637 |
960 | 0.645 |
970 | 0.652 |
980 | 0.659 |
990 | 0.667 |
1,000 | 0.674 |
1,010 | 0.681 |
1,020 | 0.689 |
1,030 | 0.696 |
1,040 | 0.703 |
1,050 | 0.710 |
1,060 | 0.717 |
1,070 | 0.724 |
1,080 | 0.730 |
1,090 | 0.737 |
λ [nm] | |
---|---|
1,100 | 0.743 |
1,110 | 0.750 |
1,120 | 0.756 |
1,130 | 0.762 |
1,140 | 0.768 |
1,150 | 0.774 |
1,160 | 0.780 |
1,170 | 0.785 |
1,180 | 0.791 |
1,190 | 0.796 |
1,200 | 0.801 |
1,250 | 0.826 |
1,300 | 0.848 |
1,350 | 0.867 |
1,400 | 0.884 |
1,450 | 0.898 |
1,500 | 0.910 |
1,550 | 0.921 |
1,600 | 0.930 |
1,650 | 0.938 |
1,700 | 0.944 |
1,750 | 0.950 |
1,800 | 0.954 |
1,850 | 0.957 |
1,900 | 0.960 |
1,950 | 0.962 |
2,000 | 0.964 |
2,050 | 0.965 |
2,100 | 0.967 |
2,150 | 0.967 |
λ [nm] | |
---|---|
2,200 | 0.963 |
2,250 | 0.962 |
2,300 | 0.962 |
2,350 | 0.963 |
2,400 | 0.962 |
2,450 | 0.958 |
2,500 | 0.955 |
2,550 | |
2,600 | |
2,650 | |
2,700 | |
2,750 | |
2,800 | |
2,850 | |
2,900 | |
2,950 | |
3,000 | |
3,050 | |
3,100 | |
3,150 | |
3,200 | |
3,250 | |
3,300 | |
3,350 | |
3,400 | |
3,450 | |
3,500 | |
3,550 | |
3,600 | |
3,650 |
λ [nm] | |
---|---|
3,700 | |
3,750 | |
3,800 | |
3,850 | |
3,900 | |
3,950 | |
4,000 | |
4,050 | |
4,100 | |
4,150 | |
4,200 | |
4,250 | |
4,300 | |
4,350 | |
4,400 | |
4,450 | |
4,500 | |
4,550 | |
4,600 | |
4,650 | |
4,700 | |
4,750 | |
4,800 | |
4,850 | |
4,900 | |
4,950 | |
5,000 | |
5,050 | |
5,100 | |
5,150 |
反射系数 | |
---|---|
Pd | 0.921 |
参考厚度 | |
---|---|
d [mm] | 1 |
承诺光谱值 | |
---|---|
τi (450nm) | ≥0.98 |
τi (633nm) | ≤0.79 |
τi (800nm) | ≤0.62 |
折射率 n |
---|
nF (486.1 nm) = 1.516 |
nh (404.7 nm) = 1.525 |
ng (435.8 nm) = 1.521 |
ns (852.1 nm) = 1.502 |
ne (546.1 nm) = 1.512 |
nd (587.6 nm) = 1.510 |
色度评估
光源 | A(Planck T = 2347K) | ||
---|---|---|---|
d [mm] | 1 | 2 | 3 |
x | |||
y | |||
Y | |||
λd [nm] | |||
Pe |
光源 | Planck T = 3200 K | ||
---|---|---|---|
d [mm] | 1 | 2 | 3 |
x | |||
y | |||
Y | |||
λd [nm] | |||
Pe |
光源 | D65 (TC = 6504 K) | ||
---|---|---|---|
d [mm] | 1 | 2 | 3 |
x | |||
y | |||
Y | |||
λd [nm] | |||
Pe |
密度 | |
---|---|
p [g/cm3] |
气泡含量 | |
---|---|
气泡等级 |
玻转温度 | |
---|---|
Tg [°C] |
温度系数 | |
---|---|
Tk [nm/°C] |
耐化学性 | |
---|---|
耐污性 | - |
耐酸性 | - |
耐碱性 | - |
热膨胀 | |
---|---|
α-30°C/+70°C [10-6/K] | |
α20°C/300°C [10-6/K] | |
α20°C/200°C [10-6/K] |