N-WG205

承诺光谱值 | |
---|---|
λc (τi = 0.5) [nm] | 205 ± 10 |
- SCHOTT
- N-WG205 - N-WG205
- 厚度
- 2.0
- 反射系数
- 0.9286
λ [nm] | |
---|---|
200 | 0.549 |
210 | 0.639 |
220 | 0.749 |
230 | 0.838 |
240 | 0.902 |
250 | 0.945 |
260 | 0.971 |
270 | 0.983 |
280 | 0.990 |
290 | 0.994 |
300 | 0.994 |
310 | 0.995 |
320 | 0.995 |
330 | 0.997 |
340 | 0.998 |
350 | 0.999 |
360 | 1.000 |
370 | 0.999 |
380 | 1.000 |
390 | 0.999 |
400 | 0.999 |
410 | 1.000 |
420 | 1.000 |
430 | 1.000 |
440 | 1.000 |
450 | 1.000 |
460 | 1.000 |
470 | 1.000 |
480 | 1.000 |
490 | 1.000 |
λ [nm] | |
---|---|
500 | 1.000 |
510 | 1.000 |
520 | 1.000 |
530 | 1.000 |
540 | 1.000 |
550 | 1.000 |
560 | 1.000 |
570 | 1.000 |
580 | 1.000 |
590 | 1.000 |
600 | 1.000 |
610 | 1.000 |
620 | 1.000 |
630 | 1.000 |
640 | 1.000 |
650 | 1.000 |
660 | 1.000 |
670 | 1.000 |
680 | 1.000 |
690 | 1.000 |
700 | 1.000 |
710 | 1.000 |
720 | 1.000 |
730 | 1.000 |
740 | 1.000 |
750 | 1.000 |
760 | 1.000 |
770 | 1.000 |
780 | 1.000 |
790 | 1.000 |
λ [nm] | |
---|---|
800 | 1.000 |
810 | 1.000 |
820 | 1.000 |
830 | 1.000 |
840 | 1.000 |
850 | 1.000 |
860 | 1.000 |
870 | 1.000 |
880 | 1.000 |
890 | 1.000 |
900 | 1.000 |
910 | 1.000 |
920 | 1.000 |
930 | 1.000 |
940 | 1.000 |
950 | 1.000 |
960 | 1.000 |
970 | 1.000 |
980 | 1.000 |
990 | 1.000 |
1,000 | 1.000 |
1,010 | 1.000 |
1,020 | 1.000 |
1,030 | 1.000 |
1,040 | 1.000 |
1,050 | 1.000 |
1,060 | 1.000 |
1,070 | 1.000 |
1,080 | 1.000 |
1,090 | 1.000 |
λ [nm] | |
---|---|
1,100 | 1.000 |
1,110 | 1.000 |
1,120 | 1.000 |
1,130 | 1.000 |
1,140 | 1.000 |
1,150 | 1.000 |
1,160 | 1.000 |
1,170 | 1.000 |
1,180 | 1.000 |
1,190 | 1.000 |
1,200 | 1.000 |
1,250 | 1.000 |
1,300 | 1.000 |
1,350 | 1.000 |
1,400 | 0.993 |
1,450 | 0.999 |
1,500 | 1.000 |
1,550 | 1.000 |
1,600 | 1.000 |
1,650 | 1.000 |
1,700 | 1.000 |
1,750 | 1.000 |
1,800 | 1.000 |
1,850 | 1.000 |
1,900 | 1.000 |
1,950 | 0.998 |
2,000 | 0.993 |
2,050 | 0.993 |
2,100 | 0.990 |
2,150 | 0.969 |
λ [nm] | |
---|---|
2,200 | 0.966 |
2,250 | 0.969 |
2,300 | 0.967 |
2,350 | 0.952 |
2,400 | 0.916 |
2,450 | 0.912 |
2,500 | 0.904 |
2,550 | 0.886 |
2,600 | 0.878 |
2,650 | 0.865 |
2,700 | 0.727 |
2,750 | 0.165 |
2,800 | 0.105 |
2,850 | 0.128 |
2,900 | 0.161 |
2,950 | 0.199 |
3,000 | 0.239 |
3,050 | 0.282 |
3,100 | 0.327 |
3,150 | 0.369 |
3,200 | 0.397 |
3,250 | 0.389 |
3,300 | 0.327 |
3,350 | 0.220 |
3,400 | 0.105 |
3,450 | 0.034 |
3,500 | 0.009 |
3,550 | 0.002 |
3,600 | < 10⁻³ |
3,650 | < 10⁻³ |
λ [nm] | |
---|---|
3,700 | 0.001 |
3,750 | 0.003 |
3,800 | 0.006 |
3,850 | 0.006 |
3,900 | 0.004 |
3,950 | 0.003 |
4,000 | 0.003 |
4,050 | 0.003 |
4,100 | 0.004 |
4,150 | 0.004 |
4,200 | 0.004 |
4,250 | 0.003 |
4,300 | 0.002 |
4,350 | 0.001 |
4,400 | < 10⁻³ |
4,450 | < 10⁻³ |
4,500 | < 10⁻³ |
4,550 | < 10⁻³ |
4,600 | < 10⁻³ |
4,650 | < 10⁻³ |
4,700 | < 10⁻³ |
4,750 | < 10⁻³ |
4,800 | < 10⁻³ |
4,850 | < 10⁻³ |
4,900 | < 10⁻³ |
4,950 | < 10⁻³ |
5,000 | < 10⁻³ |
5,050 | < 10⁻³ |
5,100 | < 10⁻³ |
5,150 | < 10⁻³ |
反射系数 | |
---|---|
Pd | 0.929 |
参考厚度 | |
---|---|
d [mm] | 2 |
承诺光谱值 | |
---|---|
λc (τi = 0.5) [nm] | 205 ± 10 |
折射率 n |
---|
nF (486.1 nm) = 1.481 |
nh (404.7 nm) = 1.489 |
ng (435.8 nm) = 1.485 |
ns (852.1 nm) = 1.470 |
ne (546.1 nm) = 1.478 |
nd (587.6 nm) = 1.476 |
色度评估
光源 | A(Planck T = 2347K) | ||
---|---|---|---|
d [mm] | 1 | 2 | 3 |
x | |||
y | |||
Y | |||
λd [nm] | |||
Pe |
光源 | Planck T = 3200 K | ||
---|---|---|---|
d [mm] | 1 | 2 | 3 |
x | |||
y | |||
Y | |||
λd [nm] | |||
Pe |
光源 | D65 (TC = 6504 K) | ||
---|---|---|---|
d [mm] | 1 | 2 | 3 |
x | |||
y | |||
Y | |||
λd [nm] | |||
Pe |
密度 | |
---|---|
p [g/cm3] | 2.22 |
气泡含量 | |
---|---|
气泡等级 | - |
玻转温度 | |
---|---|
Tg [°C] | 440 |
温度系数 | |
---|---|
Tk [nm/°C] |
耐化学性 | |
---|---|
耐污性 | - |
耐酸性 | - |
耐碱性 | - |
热膨胀 | |
---|---|
α-30°C/+70°C [10-6/K] | |
α20°C/300°C [10-6/K] | 4.1 |
α20°C/200°C [10-6/K] |