Ultra-thin glass Xensation® Flex - our first generation of glass for foldable cover solutions 

At the limit of what is physically possible! SCHOTT has managed to make the most flexible glass on earth that is produced in a melting process. Researchers from the technology group have succeeded in achieving a very small bending radius below 2 mm after processing with SCHOTT’s ultra-thin glass (UTG). This is impressive proof that Xensation® Flex is a perfect fit for foldable devices.

Discover the Innovation-Story!

Product

Foldable displays require glass that is flexible, strong and chemically toughenable. SCHOTT meets these requirements with its UTG type Xensation® Flex. A chemically toughenable aluminosilicate glass that is available in mass production thanks to the proprietary down-draw manufacturing process that has been constantly improved by SCHOTT for more than 25 years.

Key Benefits

Enabler of high quality foldable devices with premium surface.

SCHOTT Xensation® Flex advantages:
  • developed for chemical toughening
  • enabling high flexibility and small bending radius
  • excellent transparency and transmission
  • fire-polished premium surface

Product Details

Xensation® Flex is a directly hot-formed ultrathin aluminosilicate glass with excellent ion-exchange performance. After toughening, it offers a high level of bending strength and an outstanding resistance to scratches. With a bending radius below 2 mm (after processing), Xensation® Flex is produced by a draw-down process that does not require additional slimming and results in very high surface quality.
 
Stay in touch with us!

Stay in touch with us!

Home Tech, SCHOTT North America, Inc.
Xensation®
5530 Shepherdsville Road
Louisville, KY 40228
USA
SCHOTT uses Cookies on this Website to enhance the user experience and provide the best possible Service. By continuing to browse the Website, you consent to our use of Cookies.