Cover & Touch Solutions by SCHOTT

Xensation® Cover is a chemically strengthened alumino-silicate glass that offers an outstanding level of mechanical impact and bending strength, as well as high resistance to scratches. This specialty glass has been designed to achieve strength performance levels ideally suited to tough applications – from smartphone to rugged displays to automotive applications to safety glazing.

Key-Benefits of Xensation® Cover

  • Extremely high impact and bending strength for thinner, sleeker and more touch sensitive solutions
  • High scratch resistance and tolerance for superior aesthetic appeal, durability, strength and reliability even after surface damage
  • Manifold combinations of CS and DoL at the highest levels
  • Easy to process and strengthen according to accepted industry standards

Technical data of Xensation® Cover

Mechanical Properties
Density 2.477 g/cm3*
Young’s Modulus E 74 kN/mm2
Poisson’s Ratio 0.215
Shear Modulus 30 kN/mm2
Knoop Hardness HK 0.1/20  
   Non-strengthened 534
   Strengthened 639
Vickers Hardness HV 0.2/20  
   Non-strengthened 617
   Strengthened 681
Optical Properties
Refractive Index at 588 nm (nd) 633 nm 780 nm
Core Glass 1.508 1.506 1.502
Compression Layer      
   KNO3 pure 1.516 1.514 1.510
Transmittance τ  (Glass Thickness 0.7 mm)
   840 nm > 91.5 %
   560 nm > 91.5 %
   380 nm > 90 %
Photoelastic Constant 29.2 nm/cm/MPa
Typical spectral visibile light transmittance characteristics* τv
   Thickness τv
   0.55 > 92.5 %
   0.70 > 92.5 %
   1.10 > 92.4 %
   2.00 > 92.3 %

* Intergral transmittance values for the visible range of light are determined according to DIN EN 410 by using standard light type D65
Electrical Properties*
Frequency         Dielectric Constant       Loss Tangent
MHz ε´ tanδ
1 7.74 0.011
54 7.49 0.008
480 7.40 0.009
825 7.38 0.010
912 7.38 0.010
1977 7.35 0.012
2170 7.35 0.012
2986 7.34 0.012
Electric Volume Resistivity ρD for A.C. at 50Hz
at 250 °C at 350 °C  
1.5 • 106 Ω • cm     8.9 • 104 Ω • cm  

*These values are no guaranteed data - for customer orientation only.
Chemical Properties
Hydrolytic resistance acc. to DIN ISO 719         
   Hydrolytic class HGB 1
Acid resistance acc. to DIN 12116
   Acid class S 4
Alkali resistance acc. to DIN ISO 695
   Class A 1
Chemical Strengthening
Compressive Stress capable > 900 MPa
Depth of Layer capable > 100 μm
4-Point Bending Strength capable > 850 MPa
Thermal Properties
Thermal Conductivity λ (25 °C) 0.96 W/(m•K)
Specific Heat Capacity Cp (20 °C; 100 °C) 0.84 J/(g•K)
Coefficient of
Mean Linear Thermal Expansion α (20 °C; 300 °C)
8.8 • 10-6 K-1
Transformation Point Tg 615 °C
Annealing Point (1013 dPas) 635 °C
Softening Point (107.6 dPas) 880 °C
Working Point (104 dPas) 1265 °C
Forms supplied
Standard
Sheet Size: 1,150 x 850 mm
475 x 575 mm
Thickness Range: 0.55 - 2.0 mm