Broadband Infrared Ceramics for Harsh Environments

Zinc Sulfide is the most suitable material for broadband  infrared windows, domes and optics. No other material offers this combination of optical properties and environmental resistance. SCHOTT has developed a ceramic process to produce polycrystalline Zinc Sulfide, IRC-1. IRC-1 has significantly improved optical and mechanical performance compared to CVD processed material.
IRC-1
is the material of choice for mid and long wave 
IR applications


SCHOTT
can provide IRC-1 products in various custom shapes, sizes, thickness, and surface finishes. Flat
blanks, dome blanks, and curved windows can all be produced to meet each customers specific requirements.

Please download the Datasheet for more information.
empty
Exhibitions & Events
31.
March
Exhibition AIX Aircraft Interior Exposition, Hamburg, Germany, 03-31 to 04-02-2020
12.
May
Exhibition Optatec, Frankfurt, Germany, 05-12 to 05-14-2020
Contact
contact-home.png
Lighting and Imaging
SCHOTT North America Inc.

122 Charlton Street
Southbridge, MA 01550
USA
contact-phone.png
E-Mail to SCHOTT+1 (508)765-9744
SCHOTT uses Cookies on this Website to enhance the user experience and provide the best possible Service. By continuing to browse the Website, you consent to our use of Cookies.