Spectral values guaranteed
τi (405nm) =0.27± 0,03
τi (546nm) =0.31± 0,03
τi (694nm) =0.39± 0,04
Select product
SCHOTT Article
    $00.00
    Need help or a quote?
    CONTACT OUR SUPPORT
    Article Details
     
    Technical Details
    Internal Transmittance (Chart)

    Only values between 1 and 30 with one decimal place are allowed.

    Lambda [nm]
    200
    300
    400
    500
    600
    700
    800
    900
    1000
    1100
    1200
    1E-5
    1E-4
    1E-3
    0.01
    0.05
    0.1
    0.2
    0.3
    0.4
    0.5
    0.6
    0.7
    0.8
    0.9
    0.95
    0.96
    0.97
    0.98
    0.99
    SCHOTT
    NG4 - NG4
    Thickness
    1.0
    Reflection factor
    0.9223
    Internal Transmittance (Table)
    λ [nm]
    200 < 10⁻³
    210 < 10⁻³
    220 < 10⁻³
    230 < 10⁻³
    240 < 10⁻³
    250 < 10⁻³
    260 < 10⁻³
    270 < 10⁻³
    280 < 10⁻³
    290 < 10⁻³
    300 < 10⁻³
    310 < 10⁻³
    320 < 10⁻³
    330 < 10⁻³
    340 0.006
    350 0.034
    360 0.089
    370 0.139
    380 0.144
    390 0.225
    400 0.269
    410 0.275
    420 0.281
    430 0.291
    440 0.289
    450 0.302
    460 0.316
    470 0.315
    480 0.309
    490 0.302
    λ [nm]
    500 0.298
    510 0.296
    520 0.297
    530 0.301
    540 0.305
    550 0.306
    560 0.304
    570 0.298
    580 0.292
    590 0.289
    600 0.291
    610 0.297
    620 0.302
    630 0.305
    640 0.307
    650 0.309
    660 0.316
    670 0.328
    680 0.348
    690 0.369
    700 0.387
    710 0.400
    720 0.408
    730 0.412
    740 0.413
    750 0.414
    760 0.412
    770 0.409
    780 0.405
    790 0.401
    λ [nm]
    800 0.397
    810 0.392
    820 0.386
    830 0.381
    840 0.375
    850 0.368
    860 0.363
    870 0.358
    880 0.353
    890 0.347
    900 0.341
    910 0.337
    920 0.330
    930 0.325
    940 0.322
    950 0.316
    960 0.312
    970 0.308
    980 0.304
    990 0.301
    1,000 0.298
    1,010 0.296
    1,020 0.293
    1,030 0.291
    1,040 0.289
    1,050 0.288
    1,060 0.288
    1,070 0.286
    1,080 0.287
    1,090 0.286
    λ [nm]
    1,100 0.286
    1,110 0.288
    1,120 0.290
    1,130 0.292
    1,140 0.295
    1,150 0.297
    1,160 0.299
    1,170 0.302
    1,180 0.304
    1,190 0.307
    1,200 0.310
    1,250 0.328
    1,300 0.353
    1,350 0.386
    1,400 0.419
    1,450 0.452
    1,500 0.476
    1,550 0.495
    1,600 0.507
    1,650 0.512
    1,700 0.511
    1,750 0.511
    1,800 0.515
    1,850 0.522
    1,900 0.529
    1,950 0.542
    2,000 0.553
    2,050 0.566
    2,100 0.577
    2,150 0.587
    λ [nm]
    2,200 0.597
    2,250 0.608
    2,300 0.620
    2,350 0.629
    2,400 0.636
    2,450 0.642
    2,500 0.647
    2,550 0.652
    2,600 0.654
    2,650 0.653
    2,700 0.610
    2,750 0.275
    2,800 0.146
    2,850 0.132
    2,900 0.147
    2,950 0.168
    3,000 0.190
    3,050 0.218
    3,100 0.245
    3,150 0.273
    3,200 0.300
    3,250 0.326
    3,300 0.337
    3,350 0.320
    3,400 0.270
    3,450 0.205
    3,500 0.140
    3,550 0.094
    3,600 0.070
    3,650 0.056
    λ [nm]
    3,700 0.070
    3,750 0.101
    3,800 0.133
    3,850 0.154
    3,900 0.140
    3,950 0.112
    4,000 0.094
    4,050 0.090
    4,100 0.094
    4,150 0.098
    4,200 0.100
    4,250 0.093
    4,300 0.073
    4,350 0.057
    4,400 0.040
    4,450 0.025
    4,500 0.016
    4,550 0.010
    4,600 0.006
    4,650 0.004
    4,700 0.002
    4,750 0.001
    4,800 < 10⁻³
    4,850 < 10⁻³
    4,900 < 10⁻³
    4,950 < 10⁻³
    5,000 < 10⁻³
    5,050 < 10⁻³
    5,100 < 10⁻³
    5,150 < 10⁻³
    Optical values
    Reflection factor
    Pd 0.922
    Reference thickness
    d [mm] 1
    Spectral values guaranteed
    τi (405nm) =0.27± 0,03
    τi (546nm) =0.31± 0,03
    τi (694nm) =0.39± 0,04
    Refractive Indices n
    nF (486.1 nm) = 1.509
    nh (404.7 nm) = 1.517
    ng (435.8 nm) = 1.514
    ns (852.1 nm) = 1.496
    ne (546.1 nm) = 1.505
    nd (587.6 nm) = 1.503
    Colorimetric evaluation
    Illuminant A(Planck T = 2347K)
    d [mm] 1 2 3
    x
    y
    Y
    λd [nm]
    Pe
    Illuminant Planck T = 3200 K
    d [mm] 1 2 3
    x
    y
    Y
    λd [nm]
    Pe
    Illuminant D65 (TC = 6504 K)
    d [mm] 1 2 3
    x
    y
    Y
    λd [nm]
    Pe
    Physical values
    Density
    p [g/cm3] 2.4203
    Bubble content
    Bubble class 2
    Transformation temperature
    Tg [°C] 470
    Temperature coefficient
    Tk [nm/°C]
    Chemical Resistance
    FR class 1
    SR class 2.2
    AR class 1.0
    Thermal expansion
    α-30°C/+70°C [10-6/K] 6.54
    α20°C/300°C [10-6/K] 7.08
    α20°C/200°C [10-6/K]