N-BASF64

Glass Code:  704394.320

“N”-glass as an environmentally friendly alternative to conventional lead and arsenic-containing glass types.

Find more information in the tabs below or on our website.

Compare glass types with our Interactive Abbe Diagram.

optical glass klein 4zu3.jpg
Characteristics
nd 1.70400 νd 39.38
ne 1.70824 νe 39.12
nF-nC 0.017875 nF'-nC' 0.018105
Select product
SCHOTT Article
    $00.00
    Need help or a quote?
    CONTACT OUR SUPPORT
    Article Details
     
    Technical Details
    Refractive Indices
    Characteristics λ [nm]
    n2,325.4 2,325.4 1.66373
    n1,970.1 1,970.1 1.66988
    n1,529.6 1,529.6 1.67667
    n1,060.0 1,060.0 1.68453
    nt 1,014.0 1.68551
    ns 852.1 1.68982
    nr 706.5 1.69578
    nC 656.3 1.69872
    nC' 643.8 1.69955
    Characteristics λ [nm]
    n632.8 632.8 1.70033
    nD 589.3 1.70384
    nd 587.6 1.70400
    ne 546.1 1.70824
    nF 486.1 1.71659
    nF' 480.0 1.71765
    ng 435.8 1.72690
    nh 404.7 1.73581
    ni 365.0 1.75184
    Characteristics λ [nm]
    n334.1 334.1
    n312.6 312.6
    n296.7 296.7
    n280.4 280.4
    n248.3 248.3
    Internal Transmittance
    Characteristics λ [nm]
    τ25/2500 2,500 0.450
    τ25/2325 2,325 0.670
    τ25/1970 1,970 0.900
    τ25/1530 1,530 0.970
    τ25/1060 1,060 0.985
    τ25/700 700 0.970
    τ25/660 660 0.955
    τ25/620 620 0.949
    τ25/580 580 0.949
    τ25/546 546 0.950
    τ25/500 500 0.940
    τ25/460 460 0.920
    τ25/436 436 0.900
    τ25/420 420 0.880
    τ25/405 405 0.840
    τ25/400 400 0.820
    τ25/390 390 0.750
    τ25/380 380 0.610
    τ25/370 370 0.370
    τ25/365 365 0.220
    τ25/350 350
    τ25/334 334
    τ25/320 320
    τ25/310 310
    τ25/300 300
    τ25/290 290
    τ25/280 280
    τ25/270 270
    τ25/260 260
    τ25/250 250
    Characteristics λ [nm]
    τ10/2500 2,500 0.727
    τ10/2325 2,325 0.852
    τ10/1970 1,970 0.959
    τ10/1530 1,530 0.988
    τ10/1060 1,060 0.994
    τ10/700 700 0.988
    τ10/660 660 0.982
    τ10/620 620 0.979
    τ10/580 580 0.979
    τ10/546 546 0.980
    τ10/500 500 0.976
    τ10/460 460 0.967
    τ10/436 436 0.959
    τ10/420 420 0.950
    τ10/405 405 0.933
    τ10/400 400 0.924
    τ10/390 390 0.891
    τ10/380 380 0.821
    τ10/370 370 0.672
    τ10/365 365 0.546
    τ10/350 350 0.090
    τ10/334 334
    τ10/320 320
    τ10/310 310
    τ10/300 300
    τ10/290 290
    τ10/280 280
    τ10/270 270
    τ10/260 260
    τ10/250 250
    Partial Dispersion
    Characteristics
    Ps,t 0.2408
    PC,s 0.4979
    Pd,C 0.2956
    Pe,d 0.2372
    Pg,F 0.5769
    Pi,h 0.8970
    P's,t 0.2377
    P'C',s 0.5375
    P'd,C' 0.2459
    P'e,d 0.2342
    P'g,F' 0.5110
    P'i,h 0.8856
    Characteristics
    ΔPC,t 0.0069
    ΔPC,s 0.0032
    ΔPF,e -0.0004
    ΔPg,F -0.0006
    ΔPi,g 0.0012