Glass for flash lamps manufacturing

Graded seal glass rods formerly produced by Transition Glass Products TGP

In March 2017, SCHOTT AG acquired all shares of the broad portfolio of graded seal glass rods made by Transition Glass Products Ltd (“TGP”). In addition to all glass types, the entire production process as well as the quality assurance has been transferred and implemented into the SCHOTT AG, Mitterteich site.

SCHOTT Tubing offers the following glass types in rod form with intermediate expansions for graded seal applications in glass-to-glass and glass-to-metal seals, such as fused silica (quartz) to tungsten:
 
  • SCHOTT 8213, known as GS10 
    • Available Standard Sizes (Rods):
      • 2mm - 2.5mm
      • 2mm - 3mm
      • 3mm - 4mm
      • 4mm - 4.5mm
      • 4mm - 6mm
    • Standard length 1m
    • For technical details, see data sheet
    • For custom sizes, please contact us.
 
  • SCHOTT 8216, known as GS20
    • Available Standard Sizes (Rods):
      • 2 - 4 mm
    • Standard length 1m
    • For technical details please see data sheet
    • For custom sizes, please contact us.
 
  • SCHOTT 8218, known as GS25
    • Available Standard Sizes (Rods):
      • 2 - 4 mm
    • Standard length 1m
    • For technical details please see data sheet
    • For custom sizes, please contact us.
 
  • SCHOTT 8219, known as GS30 
    • Available Standard Sizes (Rods):
      • 2 - 4 mm
    • Standard length 1m
    • For technical details see data sheet
    • For custom sizes, please contact us.

For any further glass types, please see our glass tubing explorer or contact us.
Dscf7488fertig
Dscf7511fertig
Dscf7523fertig
empty

Sealing Glass Tubing

SCHOTT Tubing offers a wide range of glass tubing that is specifically developed to withstand the highest thermal exposure, such as the levels that are reached during a plasma discharge in a flash lamp. In addition our tungsten sealing glasses are manufactured to a very tight level of geometrical accuracy which allows for stable and cost-effective processing. These tight tolerances, specifically for the production of flash lamps with small dimensions, have helped to make SCHOTT Tubing the market leader.
For this application beads are also available that allow the relevant glass to be fused with electrodes.
empty
Contact
contact-home.png
Tubing
SCHOTT North America, Inc.

555 Taxter Road
Elmsford, NY 10523
USA
contact-phone.png
E-Mail to SCHOTT+1 (914)831-2200
SCHOTT uses Cookies on this Website to enhance the user experience and provide the best possible Service. By continuing to browse the Website, you consent to our use of Cookies.