Technical Details
Internal Transmittance (Chart)
- SCHOTT
- BG66 - BG66
- Thickness
- 1.0
- Reflection factor
- 0.9140
Internal Transmittance (Table)
| λ [nm] | |
|---|---|
| 200 | |
| 210 | |
| 220 | |
| 230 | |
| 240 | |
| 250 | |
| 260 | |
| 270 | |
| 280 | |
| 290 | |
| 300 | |
| 310 | |
| 320 | < 10⁻³ |
| 330 | 0.001 |
| 340 | 0.038 |
| 350 | 0.190 |
| 360 | 0.393 |
| 370 | 0.558 |
| 380 | 0.662 |
| 390 | 0.725 |
| 400 | 0.766 |
| 410 | 0.794 |
| 420 | 0.818 |
| 430 | 0.837 |
| 440 | 0.855 |
| 450 | 0.870 |
| 460 | 0.884 |
| 470 | 0.895 |
| 480 | 0.903 |
| 490 | 0.909 |
| λ [nm] | |
|---|---|
| 500 | 0.909 |
| 510 | 0.903 |
| 520 | 0.887 |
| 530 | 0.859 |
| 540 | 0.816 |
| 550 | 0.756 |
| 560 | 0.677 |
| 570 | 0.582 |
| 580 | 0.478 |
| 590 | 0.373 |
| 600 | 0.272 |
| 610 | 0.188 |
| 620 | 0.122 |
| 630 | 0.075 |
| 640 | 0.043 |
| 650 | 0.023 |
| 660 | 0.012 |
| 670 | 0.006 |
| 680 | 0.003 |
| 690 | 0.001 |
| 700 | < 10⁻³ |
| 710 | < 10⁻³ |
| 720 | < 10⁻³ |
| 730 | < 10⁻³ |
| 740 | < 10⁻³ |
| 750 | < 10⁻³ |
| 760 | < 10⁻³ |
| 770 | < 10⁻³ |
| 780 | < 10⁻³ |
| 790 | < 10⁻³ |
| λ [nm] | |
|---|---|
| 800 | < 10⁻³ |
| 810 | < 10⁻³ |
| 820 | < 10⁻³ |
| 830 | < 10⁻³ |
| 840 | < 10⁻³ |
| 850 | < 10⁻³ |
| 860 | < 10⁻³ |
| 870 | < 10⁻³ |
| 880 | < 10⁻³ |
| 890 | < 10⁻³ |
| 900 | < 10⁻³ |
| 910 | < 10⁻³ |
| 920 | < 10⁻³ |
| 930 | < 10⁻³ |
| 940 | < 10⁻³ |
| 950 | < 10⁻³ |
| 960 | < 10⁻³ |
| 970 | < 10⁻³ |
| 980 | < 10⁻³ |
| 990 | < 10⁻³ |
| 1,000 | < 10⁻³ |
| 1,010 | < 10⁻³ |
| 1,020 | < 10⁻³ |
| 1,030 | < 10⁻³ |
| 1,040 | < 10⁻³ |
| 1,050 | < 10⁻³ |
| 1,060 | < 10⁻³ |
| 1,070 | < 10⁻³ |
| 1,080 | < 10⁻³ |
| 1,090 | < 10⁻³ |
| λ [nm] | |
|---|---|
| 1,100 | < 10⁻³ |
| 1,110 | < 10⁻³ |
| 1,120 | < 10⁻³ |
| 1,130 | < 10⁻³ |
| 1,140 | < 10⁻³ |
| 1,150 | < 10⁻³ |
| 1,160 | < 10⁻³ |
| 1,170 | 0.001 |
| 1,180 | 0.001 |
| 1,190 | 0.002 |
| 1,200 | 0.002 |
| 1,250 | 0.006 |
| 1,300 | 0.015 |
| 1,350 | 0.032 |
| 1,400 | 0.060 |
| 1,450 | 0.101 |
| 1,500 | 0.154 |
| 1,550 | 0.219 |
| 1,600 | 0.291 |
| 1,650 | 0.366 |
| 1,700 | 0.432 |
| 1,750 | 0.500 |
| 1,800 | 0.562 |
| 1,850 | 0.619 |
| 1,900 | 0.668 |
| 1,950 | 0.713 |
| 2,000 | 0.750 |
| 2,050 | 0.781 |
| 2,100 | 0.810 |
| 2,150 | 0.832 |
| λ [nm] | |
|---|---|
| 2,200 | 0.851 |
| 2,250 | 0.868 |
| 2,300 | 0.881 |
| 2,350 | 0.893 |
| 2,400 | 0.903 |
| 2,450 | 0.911 |
| 2,500 | 0.917 |
| 2,550 | 0.921 |
| 2,600 | 0.924 |
| 2,650 | 0.926 |
| 2,700 | 0.925 |
| 2,750 | 0.919 |
| 2,800 | 0.888 |
| 2,850 | 0.833 |
| 2,900 | 0.780 |
| 2,950 | 0.739 |
| 3,000 | 0.703 |
| 3,050 | 0.671 |
| 3,100 | 0.639 |
| 3,150 | 0.608 |
| 3,200 | 0.580 |
| 3,250 | 0.555 |
| 3,300 | 0.534 |
| 3,350 | 0.518 |
| 3,400 | 0.504 |
| 3,450 | 0.496 |
| 3,500 | 0.493 |
| 3,550 | 0.495 |
| 3,600 | 0.502 |
| 3,650 | 0.514 |
| λ [nm] | |
|---|---|
| 3,700 | 0.530 |
| 3,750 | 0.541 |
| 3,800 | 0.535 |
| 3,850 | 0.498 |
| 3,900 | 0.437 |
| 3,950 | 0.370 |
| 4,000 | 0.291 |
| 4,050 | 0.196 |
| 4,100 | 0.109 |
| 4,150 | 0.056 |
| 4,200 | 0.030 |
| 4,250 | 0.018 |
| 4,300 | 0.016 |
| 4,350 | 0.017 |
| 4,400 | 0.015 |
| 4,450 | 0.012 |
| 4,500 | 0.009 |
| 4,550 | 0.007 |
| 4,600 | 0.007 |
| 4,650 | 0.008 |
| 4,700 | 0.013 |
| 4,750 | 0.022 |
| 4,800 | 0.033 |
| 4,850 | 0.048 |
| 4,900 | 0.066 |
| 4,950 | 0.091 |
| 5,000 | 0.120 |
| 5,050 | 0.149 |
| 5,100 | 0.171 |
| 5,150 | 0.181 |
Optical values
| Reflection factor | |
|---|---|
| Pd | 0.914 |
| Reference thickness | |
|---|---|
| d [mm] | 1 |
| Spectral values guaranteed | |
|---|---|
| τi (514nm) | ≥0.89 |
| τi (694nm) | ≤0.0015 |
| τi (1060nm) | ≤0.0002 |
| Refractive Indices n |
|---|
| nF (486.1 nm) = 1.544 |
| nh (404.7 nm) = 1.552 |
| ng (435.8 nm) = 1.549 |
| ns (852.1 nm) = 1.532 |
| ne (546.1 nm) = 1.541 |
| nd (587.6 nm) = 1.539 |
Colorimetric evaluation
| Illuminant | A(Planck T = 2347K) | ||
|---|---|---|---|
| d [mm] | 1 | 2 | 3 |
| x | 0.303 | 0.237 | 0.202 |
| y | 0.440 | 0.438 | 0.429 |
| Y | 48 | 33 | 25 |
| λd [nm] | 499 | 497 | 496 |
| Pe | 0.33 | 0.49 | 0.57 |
| Illuminant | Planck T = 3200 K | ||
|---|---|---|---|
| d [mm] | 1 | 2 | 3 |
| x | 0.285 | 0.225 | 0.193 |
| y | 0.419 | 0.412 | 0.401 |
| Y | 50 | 34 | 26 |
| λd [nm] | 497 | 495 | 495 |
| Pe | 0.34 | 0.49 | 0.58 |
| Illuminant | D65 (TC = 6504 K) | ||
|---|---|---|---|
| d [mm] | 1 | 2 | 3 |
| x | 0.218 | 0.183 | 0.165 |
| y | 0.313 | 0.297 | 0.286 |
| Y | 57 | 42 | 33 |
| λd [nm] | 489 | 489 | 488 |
| Pe | 0.36 | 0.50 | 0.57 |
Physical values
| Density | |
|---|---|
| p [g/cm3] | 2.8512 |
| Bubble content | |
|---|---|
| Bubble class | |
| Transformation temperature | |
|---|---|
| Tg [°C] | 416 |
| Temperature coefficient | |
|---|---|
| Tk [nm/°C] | |
| Chemical Resistance | |
|---|---|
| FR class | |
| SR class | 52.3 |
| AR class | 3.3 |
| Thermal expansion | |
|---|---|
| α-30°C/+70°C [10-6/K] | 11.78 |
| α20°C/300°C [10-6/K] | 13.66 |
| α20°C/200°C [10-6/K] | |