SF6G05  809253.520

optical glass klein 4zu3.jpg
SCHOTT Advanced Optics offers a variety of radiation resistant glass types with different dispersion properties. These glass types are well-suited to use in surroundings with high radioactivity.
Characteristics
nd 1.80906 νd 25.28
ne 1.81661 νe 25.08
nF-nC 0.032015 nF'-nC' 0.032570
Characteristics λ [nm]
n2,325.4 2,325.4 1.75661
n1,970.1 1,970.1 1.76163
n1,529.6 1,529.6 1.76797
n1,060.0 1,060.0 1.77741
nt 1,014.0 1.77879
ns 852.1 1.78524
nr 706.5 1.79491
nC 656.3 1.79988
nC' 643.8 1.80131
Characteristics λ [nm]
n632.8 632.8 1.80265
nD 589.3 1.80878
nd 587.6 1.80906
ne 546.1 1.81661
nF 486.1 1.83190
nF' 480.0 1.83387
ng 435.8
nh 404.7
ni 365.0
Characteristics λ [nm]
n334.1 334.1
n312.6 312.6
n296.7 296.7
n280.4 280.4
n248.3 248.3
Characteristics λ [nm]
τ25/2500 2,500 0.660
τ25/2325 2,325 0.721
τ25/1970 1,970 0.915
τ25/1530 1,530 0.987
τ25/1060 1,060 0.994
τ25/700 700 0.962
τ25/660 660 0.950
τ25/620 620 0.931
τ25/580 580 0.898
τ25/546 546 0.805
τ25/500 500 0.330
τ25/460 460 0.080
τ25/436 436
τ25/420 420
τ25/405 405
τ25/400 400
τ25/390 390
τ25/380 380
τ25/370 370
τ25/365 365
τ25/350 350
τ25/334 334
τ25/320 320
τ25/310 310
τ25/300 300
τ25/290 290
τ25/280 280
τ25/270 270
τ25/260 260
τ25/250 250
Characteristics λ [nm]
τ10/2500 2,500 0.847
τ10/2325 2,325 0.877
τ10/1970 1,970 0.965
τ10/1530 1,530 0.995
τ10/1060 1,060 0.998
τ10/700 700 0.985
τ10/660 660 0.980
τ10/620 620 0.972
τ10/580 580 0.958
τ10/546 546 0.917
τ10/500 500 0.642
τ10/460 460 0.090
τ10/436 436
τ10/420 420
τ10/405 405
τ10/400 400
τ10/390 390
τ10/380 380
τ10/370 370
τ10/365 365
τ10/350 350
τ10/334 334
τ10/320 320
τ10/310 310
τ10/300 300
τ10/290 290
τ10/280 280
τ10/270 270
τ10/260 260
τ10/250 250
Characteristics
Ps,t 0.2013
PC,s 0.4574
Pd,C 0.2866
Pe,d 0.2358
Pg,F
Pi,h
P's,t 0.1979
P'C',s 0.4933
P'd,C' 0.2380
P'e,d 0.2318
P'g,F'
P'i,h
Characteristics
ΔPC,t -0.0062
ΔPC,s -0.0044
ΔPF,e 0.0025
ΔPg,F
ΔPi,g